Original language | Dutch |
---|---|
Pages (from-to) | 105 - 111 |
Number of pages | 10 |
Journal | Surface Engineering |
Volume | 17 |
Issue number | 2 |
DOIs | |
Publication status | Published - 2001 |
Keywords
- COATED SYSTEMS
- ELASTIC-MODULUS
- CONTACT AREA
- INDENTATION
- HARDNESS
- CARBON
- LOAD
N.J.M. Carvalho, J.T.M. de Hosson
Research output: Contribution to journal › Article › Academic › peer-review
Original language | Dutch |
---|---|
Pages (from-to) | 105 - 111 |
Number of pages | 10 |
Journal | Surface Engineering |
Volume | 17 |
Issue number | 2 |
DOIs | |
Publication status | Published - 2001 |